Improved homing cycle has led to (near) perfect registration of solder mask.
Layer registration mark, lines are ~0.1mm wide.
Part of TSSOP 20 footprint, mask is way past "use before" date so some problems with spots appearing.
I have started to apply the Riston film on wet PCBs, dust problem nearly gone - easier to handle.
Terje